Common Ion Effect in Anaerobic Corrosion of Metals 金属厌氧腐蚀中的同离子效应
In the first stage, anaerobic hydrogen depolarization is predominant and produced iron oxide corrosion product layer; 初期是厌氧条件下的氢去极化,生成氧化物产物层;
The results show that there exists a so-called common ion effect, that is, these metal ions can stimulate the anaerobic corrosion of the corresponding metals. 结果表明,这些金属离子会促进相应的金属腐蚀,即表现出同离子效应。